| No. of walls | 7 walls |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80-2.50 N/mm2 |
| Weight | 9.0 – 10 Kg |
| Thermal Conductivity | 0.15 W/mk |
| Sound Reflection Ratio | 88% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 5 walls |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80-2.40 N/mm2 |
| Weight | 9.0 – 10 Kg |
| Thermal Conductivity | 0.16 W/mk |
| Sound Reflection Ratio | 87% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 5 walls |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80-2.40 N/mm2 |
| Weight | 9.0 – 10 Kg |
| Thermal Conductivity | 0.16 W/mk |
| Sound Reflection Ratio | 87% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 3 walls |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80-2.40 N/mm2 |
| Weight | 7.0 – 8.0 Kg |
| Thermal Conductivity | 0.18 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 3 walls |
| Depth | 15 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80-2.40 N/mm2 |
| Weight | 6.0 – 7.0 Kg |
| Thermal Conductivity | 0.18 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 5 walls |
| Depth | 15 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80-2.50 N/mm2 |
| Weight | 7.0 – 8.0 Kg |
| Thermal Conductivity | 0.18 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 4 walls |
| Depth | 15 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.50-2.50 N/mm2 |
| Weight | 6.0 – 8.0 Kg |
| Thermal Conductivity | 0.18 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 2 walls |
| Depth | 12 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.60 - 2.00 N/mm2 |
| Weight | 5.0 – 6.0 Kg |
| Thermal Conductivity | 0.17 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 2 walls |
| Depth | 12 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.60-2.00 N/mm2 |
| Weight | 5.0 – 6.0 Kg |
| Thermal Conductivity | 0.17 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 2 walls |
| Depth | 10 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.60-2.00 N/mm2 |
| Weight | 5.0 – 6.0 Kg |
| Thermal Conductivity | 0.17 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 3 walls |
| Depth | 10 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.60-2.00 N/mm2 |
| Weight | 5.0 – 6.0 Kg |
| Thermal Conductivity | 0.16 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 4 walls |
| Depth | 25 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.60-2.00 N/mm2 |
| Weight | 9.0 – 11 Kg |
| Thermal Conductivity | 0.16 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 5 walls |
| Depth | 30 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 2.0 – 3.0 N/mm2 |
| Weight | 10.5 – 11.5 Kg |
| Thermal Conductivity | 0.14 W/mk |
| Sound Reflection Ratio | 90% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 3 walls |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.4 - 2.0 N/mm2 |
| Weight | 6.5 – 7.5 Kg |
| Thermal Conductivity | 0.18 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 3 walls |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 5.0 – 9.0 N/mm2 |
| Weight | 13.5 – 15.0 Kg |
| Thermal Conductivity | 0.13 W/mk |
| Sound Reflection Ratio | 92% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| No. of walls | 4 walls + 3 cm Flin |
| Depth | 19 cm |
| Hight | 19 cm |
| Length | 39 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 1.80 - 2.50 N/mm2 |
| Weight | 8.0 – 10.0 Kg |
| Thermal Conductivity | 0.18 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| Type Q | |
|---|---|
| No. of walls | 3 walls |
| Depth | 20 cm |
| Hight | 20 cm |
| Length | 40 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 5.0 – 9.0 N/mm2 |
| Weight | 15.0 – 17.0 Kg |
| Thermal Conductivity | 0.13 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| Type R | |
|---|---|
| No. of walls | 3 walls |
| Depth | 25 cm |
| Hight | 20 cm |
| Length | 40 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 5.0 – 9.0 N/mm2 |
| Weight | 17.0 – 19.0 Kg |
| Thermal Conductivity | 0.13 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |
| Type S | |
|---|---|
| No. of walls | 3 walls |
| Depth | 15 cm |
| Hight | 20 cm |
| Length | 40 cm |
| Volume Changing Ratio | ±2% |
| Compressive Strength | 5.0 – 8.0 N/mm2 |
| Weight | 9.0 – 11.0 Kg |
| Thermal Conductivity | 0.13 W/mk |
| Sound Reflection Ratio | 85% |
| Fire Resistance | A1 |
| Water Evaporation Ratio | 9.5 Kgm2 Sp |